Item type |
[ELS]紀要論文 / Departmental Bulletin Paper(1) |
公開日 |
2016-07-25 |
タイトル |
|
|
タイトル |
大島紬の燃焼性の研究 |
タイトル |
|
|
タイトル |
Flammability of Oshima-Tsumugi |
|
言語 |
en |
言語 |
|
|
言語 |
jpn |
資源タイプ |
|
|
資源タイプ識別子 |
http://purl.org/coar/resource_type/c_6501 |
|
資源タイプ |
departmental bulletin paper |
雑誌書誌ID |
|
|
収録物識別子タイプ |
NCID |
|
収録物識別子 |
AN00039943 |
論文名よみ |
|
|
タイトル |
〓 |
著者 |
石橋, 博
村田, 博司
ISHIBASHI, Hiroshi
MURATA, Hiroshi
|
抄録(英) |
|
|
内容記述タイプ |
Other |
|
内容記述 |
Flammability of the Oshima-Tsumugi was evaluated with Mushroom Apparel Flammability test, DOC FF 3-71 test, JIS L 1O91 A-4 test and Oxygen Index test. Mud mordanting was found to effect an increase in the flame retardancy of silk. The mud-dyed Oshima-Tsumugi did not propagate flame but char on exposure to flames and meet the severe requirements of the framed vertical strip test DOC FF 3-71 and JIS L 1091 A-4. The Oxygen Index value of the mud-dyed Oshima-Tsumugi is 27.7~28.5 which is sufficient to meet a vertical flame test. From the results of atomic absorption analysis, thermal analysis (DTA, TG) and scanning electron microscopy of the Oshima-Tsumugi, the flame resistance of the mud-dyed Oshima-Tsumugi is presumed to be due to the charring-promoting effect of iron salt during the pyrolysis of silk and the covering effect of surface deposition of calcium tannate and clay. |