抄録(英) |
|
|
内容記述タイプ |
Other |
|
内容記述 |
Exposing woven goods dyed with direct, basic, acid, sulphur, acid mordant, ice and vat colors to the sun, with standard blue scale dyed goods, the author of this paper judged their durability comparing the fading of color of both of them. At the test it was found that most dyed fabrics were faded due to their exposure to the sun while those dyed with vat and acid mordant colors retained their durability very excellently and no change of fading was noticed showing the durability of 7-8 grade. Among vat colors, colors of threne group revealed higher durability than those of indigo group. On the other hand ice and sulphur colors showed their durability of 4-5 grade and acid, direct and basic colors followed their declining order of durability. Acid colors brought about striking drop of durability on account of the spectrum difference. Among direct colors direct copper blue revealed its fading comparatively later, particularly those treated with metalic salts revealed improving its durability up to 5 grade. The test above was practised in Tokyo simultaneously with the same stuff and it was found that in Kagoshima they faded away in far shorter period. |
書誌情報 |
巻 10,
p. 36_a-31_a,
発行日 1960-01-25
|
表示順 |
|
|
内容記述タイプ |
Other |
|
内容記述 |
10 |
アクセション番号 |
|
|
内容記述タイプ |
Other |
|
内容記述 |
KJ00002126242 |